Majority of new TTC streetcars recalled over welding defect
Videos
-
Majority of new TTC streetcars recalled over welding defect02:09 | July 4, 2018 -
What to know before you purchase a vehicle04:37 | July 31, 2026 -
Margaret Atwood’s work at the National Ballet of Canada03:46 | June 16, 2026 -
World Cup: Five Team Canada players call Brampton home04:39 | June 5, 2026 -
Organizing your garage during spring cleaning05:18 | May 21, 2026 -
Opening Day: Blue Jays baseball returns to Rogers Centre01:59 | March 27, 2026 -
Step inside the ISS at ‘Space Explorers: THE INFINITE’ in Mississauga07:46 | March 16, 2026 -
Municipal Matters: World Cup Countdown05:25 | March 5, 2026 -
Emerging home trends for 202604:48 | March 4, 2026 -
Raising awareness around women’s health05:37 | March 4, 2026 -
Keep orchids thriving05:25 | March 4, 2026 -
World talent showcased at the Toronto Black Film Festival04:17 | February 13, 2026 -
Creative crafts for Valentine’s Day05:38 | February 13, 2026 -
Sweet treats for Valentine’s Day and Family Day05:46 | February 13, 2026 -
Toronto Blue Jays prepare to celebrate 50th season05:20 | February 12, 2026 -
Sweet and savoury foods with chocolate for Valentine’s Day05:20 | February 12, 2026 -
1 man shot outside Woodbridge home, suspects flee in Porsche02:01 | January 21, 2026 -
3 injured, 1 unaccounted for in Oshawa house fire01:38 | January 20, 2026 -
‘They didn’t sound like fireworks’: Neighbours recall police-involved shooting in Oshawa01:53 | January 19, 2026 -
Snowplows and budgets: A conversation with Mayor Olivia Chow04:40 | January 16, 2026 -
Planning summer camp options05:00 | January 16, 2026 -
De-icing salt alternatives for your home05:03 | January 16, 2026 -
Footage captures tow truck lit on fire in Brampton01:54 | January 13, 2026 -
More service disruptions to Finch West LRT01:33 | January 12, 2026 -
Eglinton LRT to open ‘early in February’: Ford02:02 | January 9, 2026 -
City proposes 2.2% tax increase in 2026 Toronto budget02:04 | January 8, 2026 -
Greater Toronto Area bracing for ice storm02:23 | January 6, 2026 -
Suspected arson at Brampton tow truck company under investigation01:20 | January 5, 2026 -
Residents displaced in apartment fire on Eglinton Avenue East01:44 | December 18, 2025 -
Pearson prepares for busiest travel season of the year01:55 | December 17, 2025 -
‘Unprecedented’ fire in Thorncliffe Park finally extinguished01:52 | December 16, 2025 -
‘A more sombre Hannukah’ local Jewish leaders react to Australian terror attack01:44 | December 15, 2025
-
Majority of new TTC streetcars recalled over welding defect02:09 | July 4, 2018
-
What to know before you purchase a vehicle04:37 | July 31, 2026
-
Margaret Atwood’s work at the National Ballet of Canada03:46 | June 16, 2026
-
World Cup: Five Team Canada players call Brampton home04:39 | June 5, 2026
-
Organizing your garage during spring cleaning05:18 | May 21, 2026
-
Opening Day: Blue Jays baseball returns to Rogers Centre01:59 | March 27, 2026
-
Step inside the ISS at ‘Space Explorers: THE INFINITE’ in Mississauga07:46 | March 16, 2026
-
Municipal Matters: World Cup Countdown05:25 | March 5, 2026
-
Emerging home trends for 202604:48 | March 4, 2026
-
Raising awareness around women’s health05:37 | March 4, 2026
-
Keep orchids thriving05:25 | March 4, 2026
-
World talent showcased at the Toronto Black Film Festival04:17 | February 13, 2026
-
Creative crafts for Valentine’s Day05:38 | February 13, 2026
-
Sweet treats for Valentine’s Day and Family Day05:46 | February 13, 2026
-
Toronto Blue Jays prepare to celebrate 50th season05:20 | February 12, 2026
-
Sweet and savoury foods with chocolate for Valentine’s Day05:20 | February 12, 2026
-
1 man shot outside Woodbridge home, suspects flee in Porsche02:01 | January 21, 2026
-
3 injured, 1 unaccounted for in Oshawa house fire01:38 | January 20, 2026
-
‘They didn’t sound like fireworks’: Neighbours recall police-involved shooting in Oshawa01:53 | January 19, 2026
-
Snowplows and budgets: A conversation with Mayor Olivia Chow04:40 | January 16, 2026
-
Planning summer camp options05:00 | January 16, 2026
-
De-icing salt alternatives for your home05:03 | January 16, 2026
-
Footage captures tow truck lit on fire in Brampton01:54 | January 13, 2026
-
More service disruptions to Finch West LRT01:33 | January 12, 2026
-
Eglinton LRT to open ‘early in February’: Ford02:02 | January 9, 2026
-
City proposes 2.2% tax increase in 2026 Toronto budget02:04 | January 8, 2026
-
Greater Toronto Area bracing for ice storm02:23 | January 6, 2026
-
Suspected arson at Brampton tow truck company under investigation01:20 | January 5, 2026
-
Residents displaced in apartment fire on Eglinton Avenue East01:44 | December 18, 2025
-
Pearson prepares for busiest travel season of the year01:55 | December 17, 2025
-
‘Unprecedented’ fire in Thorncliffe Park finally extinguished01:52 | December 16, 2025
-
‘A more sombre Hannukah’ local Jewish leaders react to Australian terror attack01:44 | December 15, 2025
Majority of new TTC streetcars recalled over welding defect
Description
July 4, 2018
Sixty-seven of the 89 new TTC streetcars already on city streets are heading back to the factory for repairs. Shallima Maharaj explains.
National News
-
NATO jet downs suspected Russian drone over Lithuania1:5215 hours ago -
SCOTUS pushes back against Trump ahead of midterm elections1:5715 hours ago -
Alberta NDP upsets UCP stronghold in byelection2:0115 hours ago -
Carney heads to Europe aiming to build ‘unique alliance’ with EU2:1215 hours ago -
Carney to open Canada’s 4 largest airports to private investment2:3115 hours ago -
Global National: Sept. 1519:0916 hours ago -
Nick Reiner will not receive death penalty in parents’ murders, says district attorney0:5915 hours ago -
NDP byelection win in historically conservative Calgary riding reflects referendum sentiments: Analysts1:5515 hours ago -
Girl gets run over by dump truck, makes it out with only a few scrapes1:0618 hours ago -
Stephen Harper believes Canada had ‘no choice’ but to walk away from US trade talks1:1019 hours ago
Advertisement
Top News
-
NATO jet downs suspected Russian drone over Lithuania1:5215 hours ago -
Alberta NDP upsets UCP stronghold in byelection2:0115 hours ago -
Court appearance for Calgary man charged with threats against Prime Minister Carney1:5015 hours ago -
Carney announces airport private investment plan3:3015 hours ago -
Mark Carney opening 4 Canadian airports to private investment2:4615 hours ago -
2026 Emmy Awards: The hottest celebrity looks from the red carpet5:2322 hours ago -
Record-high diesel prices spark fears of higher grocery costs1:4722 hours ago -
BC’s deficit grows to $13.8B2:102 days ago -
Data centre biggest Sask. investment in history1:412 days ago -
Passenger ferry capsizes in Indonesia’s Java Sea, killing at least 61:572 days ago
Sponsored Content
Global National
-
Global National: Sept. 1519:0916 hours ago -
Global National: Sept. 1422:102 days ago -
Global National: Sept. 1322:153 days ago -
Global National: Sept. 1221:394 days ago -
Global National: Sept. 1122:515 days ago -
Global National: Sept. 1022:206 days ago -
Global National: Sept. 921:327 days ago -
Global National: Sept. 822:391 week ago -
Global National: Sept. 721:571 week ago -
Global National: Sept. 621:571 week ago
Trending
-
Young Toronto entertainer brings classic jazz pop to a new generation3:041 week ago -
Canadian broadcasting legend Lloyd Robertson dies at 923:311 month ago
-
1 dead after cooking-related fire at Toronto apartment building2:301 month ago -
Olivia Chow finally confirms she’s running for a second term at Toronto’s Mayor2:294 months ago -
Toronto fire crews melt Drake ice sculpture2:165 months ago -
Toronto man who killed 2 strangers 2 days apart found guilty of first-degree murder2:063 months ago -
Toronto kicks-off spring cleanup campaign1:395 months ago -
Toronto man found guilty of murdering husband in 20212:053 months ago -
U.S. consulate in Toronto hit by gunfire, police declare national security incident1:516 months ago -
Metrolinx sheds 400-plus consultants, some move to become VPs3:536 months ago
Canada
-
Carney heads to Europe aiming to build ‘unique alliance’ with EU2:1215 hours ago -
Carney to open Canada’s 4 largest airports to private investment2:3115 hours ago -
Carney announces airport private investment plan3:3015 hours ago -
Calgary among airports primed for privatization2:0115 hours ago -
Mark Carney opening 4 Canadian airports to private investment2:4615 hours ago -
Longtime Conservative riding Calgary-Shaw flips orange with NDP win1:5222 hours ago -
‘If it doesn’t save money, why do it?’: Poilievre on Carney seeking private investments at airports1:0422 hours ago -
Carney makes several economic announcements during keynote address at Toronto investment summit8:3422 hours ago -
Canada’s inflation rate steady at 3% in August as travel costs soar2:0122 hours ago -
Carney pitches projects at inaugural Canada Investment Summit2:062 days ago
U.S. News
-
SCOTUS pushes back against Trump ahead of midterm elections1:5715 hours ago -
U.S. announces space-based weapons: What’s the risk?2:0520 hours ago -
Bernie Sanders, Steve Bannon demand AI restrictions at ‘pro-human’ summit1:5715 hours ago -
Business Matters: Select Canadian goods hit by new U.S. tariffs2:1622 hours ago -
Bob Mackie, legendary fashion designer, dies at 871:5922 hours ago -
‘SICK conspiracy’: Trump dismisses growing concerns about AI risks to humanity2:0022 hours ago -
Sydney Sweeney sports betting ad faces mounting backlash1:542 days ago -
‘I find Canada to be the worst country to deal with,’ Trump tells reporters0:292 days ago -
Trump downplays AI warnings as concerns grow2:342 days ago -
U.S.-Canada trade war makes cross-border shipping tougher5:353 days ago
Advertisement
World
-
NATO jet downs suspected Russian drone over Lithuania1:5215 hours ago -
Conflict with U.S. and Iran causing changes to Dalhousie law school admission process2:1415 hours ago -
‘SICK conspiracy’: Trump dismisses growing concerns about AI risks to humanity2:0022 hours ago -
What Carney’s push to strengthen Canada-EU ties could look like2:0122 hours ago -
Record-high diesel prices spark fears of higher grocery costs1:4722 hours ago -
Passenger ferry capsizes in Indonesia’s Java Sea, killing at least 61:572 days ago -
Celine Dion returns to the stage after 6 years at Paris residency: ‘I missed this’2:022 days ago -
Trump says he would ‘love’ to see Ireland unified2:183 days ago -
9/11, 25 years later: Remembering Rick Rescorla, who saved thousands of lives, but lost his own3:035 days ago -
Israel destroys Hezbollah tunnels in southern Lebanon1:425 days ago
Politics
-
EU prepared to make Canada ‘associate member,’ but what does that mean?2:084 hours ago -
NATO jet downs suspected Russian drone over Lithuania1:5215 hours ago -
SCOTUS pushes back against Trump ahead of midterm elections1:5715 hours ago -
Alberta NDP upsets UCP stronghold in byelection2:0115 hours ago -
Carney heads to Europe aiming to build ‘unique alliance’ with EU2:1215 hours ago -
Carney to open Canada’s 4 largest airports to private investment2:3115 hours ago -
Court appearance for Calgary man charged with threats against Prime Minister Carney1:5015 hours ago -
Carney announces airport private investment plan3:3015 hours ago -
Calgary-Shaw voters flip conservative stronghold, elect NDP’s Kyle Campbell in byelection1:5515 hours ago -
New Ipsos poll shows support for BC Conservatives dropping under new leader2:0517 hours ago
Health and Wellness
-
Montreal father, daughter turn cancer diagnosis into push for awareness2:4522 hours ago -
RSV immunization reduces infant ICU admissions by 97%, study says1:4422 hours ago -
Health Matters: AB government maintaining $100 COVID-19 vaccine fee2:1222 hours ago -
Nova Scotia unveils initatives to improve women’s health care2:062 days ago -
Endometrial cancer awareness campaign kicks off, doctors say more education needed1:322 days ago -
Health Matters: 3 deaths in Pennsylvania associated with measles outbreak, records show2:142 days ago -
Vaccine-injured Canadians testify in Ottawa2:202 days ago -
Generic acetaminophen tablets recalled across Canada0:355 days ago -
Study finds drug seizures increased during decriminalization pilot4:005 days ago -
Health Matters: Ottawa announces $5M in funding to support HIV prevention and support services1:565 days ago
Advertisement
Investigative News
-
Study finds drug seizures increased during decriminalization pilot4:005 days ago -
Questions about Vancouver police investigation into Kal Dosanjh2:121 week ago -
Why would NASA researchers be interested in studying the Pear Lake fire the Cariboo? And why was a Cold War era plane used to fly over it?6:341 week ago -
Canada gave contracts to Iran VP’s son while investigating role in regime missile program2:462 weeks ago -
Global exclusive: Richmond kidnapping update2:262 months ago -
FOI requests reveal Saskatchewan man’s foster system abuse claims were documented, then ignored3:242 months ago -
‘Operation Hard Ball’ suspects in court2:242 months ago -
The expanding reach of India-based organized crime groups in Canada4:452 months ago -
Stranger attack victim speaks out after release of suspect2:312 months ago -
Why Carleton University student has been flagged as a security threat2:103 months ago
News Bloopers
-
Atlantic Canadian politicians react after Hilroy leaves Cape Breton, Newfoundland off its cover2:052 weeks ago -
‘Amoosing’ cow leaves Global News Morning crew in stitches1:599 months ago -
‘Can’t use that on TV’: Watch a Global News reporter jump from the highest bungee jump in Canada0:3717 months ago -
Edmonton, B.C. morning show hosts settle NHL playoff bet3:0528 months ago -
‘You can’t make this stuff up:’ Loud clap of thunder interrupts live TV segment at pivotal moment0:2535 months ago -
Global Calgary weather anchor startled by surprise guest appearance0:2139 months ago -
‘Buzzworthy moment’: Colin D’Mello recaps Doug Ford accidentally swallowing a bee1:5749 months ago -
‘Did you just call me daddy?’: Morning show hosts can’t hold back laughter after on-air mixup1:1550 months ago -
B.C. dad hoping to see his cloud photo on TV get his wish following viral TikTok campaign2:1253 months ago -
Bloopers: Phil Darlington slips, slides and falls in these Our Winter City outtakes1:3847 months ago